Asking for input from #FusedGlass or other #Kiln artists. I had a strange result...
(HistorySheWrote) has moved @bethroots@mindly.social
Asking for input from #FusedGlass or other #Kiln artists.
I had a strange result from a schedule change. I added a 15-minute hold in the middle of the schedule, but it ran only 10 minutes more than the prior run, rather than 15 minutes more. I have an idea but would really like other ideas or feedback. This is testing small pieces, so no annealing.
Small jewelry kiln, 6x6x4, firebrick, side element, clay shelf, 3 button controller.
First run AFAP to 1420F hold 15, Off. Started at 77F and ran 43 minutes. Glass red, opaline, clear. Papyros.
Second run AFAP to 1000F hold 15, AFAP to 1420F hold 15, Off. Started at 76F and ran 53 minutes. Glass clear, opaline. Thinfire.
My thoughts:
1. The extra hold at 1000F stabilized the heat and assured the shelf was hot, so it was easier and faster to get to final temp.
2. The red glass absorbed more of the heat in run one, making the run slower than the second. However, this theory doesn't seem to be able to account for 5 minutes.
Anybody?