A lot of folks suggest annealing PA6-CF for 8+hrs at temps ranging from 80C to 1...
xssfox (crossy) @xssfox@cloudisland.nz
A lot of folks suggest annealing PA6-CF for 8+hrs at temps ranging from 80C to 120C. But it seems that's nearly entirely pointless.
It seems you want 170C. Time plays very little into it and just 2hrs is probably enough.
> From the tests conducted it can be concluded that if one wants to increase the mechanical properties, primarily strength and modulus, it is necessary to go to much higher temperatures, and that temperatures of 80 -120 °C as in these previous studies are not sufficient for improvement. The time of even 8 hours mentioned by the author Bhandari, S. et al. [14] is not necessary because time has no effect on the entire tensile properties what this research showed (all p-values > 0.5).